>>How do I make Ionic/ Colloidal Silver using the heat method?
Bring 2 cups of distilled water to the boil in a nonmetal container. Pour into a glass jar and immerse about 75% of the silver wires. Let the unit run for 15 to 20 minutes for 5-8 PPM . The water is brought to the boil simply to give a standard for heat. Heating is necessary to increase the conductivity of the water.<<
http://www.sotainstruments.com/original/documents/faqs.html
So are we talking about a microwave?? (
Also - I'd like make a higher PPM. Is this possibly only via the heat method? Can someone describe how, if not a microwave, one boils water in a non metalic container? Do I need a glass pot, ceramic? What are we using here?